N2 - High-temperature coatings are routinely exposed to pre-existing surface damage, yet their ability to sustain sliding contact after such damage remains insufficiently quantified. This study develops a damage-tolerant reliability-mapping workflow for AlCrN coatings deposited by physical vapour deposition (PVD), based on intersecting controlled pre-scratch defects with dry sliding contact at room temperature, 500 °C and 800 °C. A multilayer AlCrN coating on austenitic Cr-Ni-steel (253 MA) was first damaged by calibrated constant-load scratching (1.96–16.67 N) and then subjected to ball-on-disc sliding over an equivalent load range (temperature-dependent initial elastic Hertzian reference pressure 0.78–1.95 GPa). Surface responses at the scratch–wear intersections were classified using an 18-event taxonomy and reduced to a scalar reliability index; conservative monotone safe envelopes were then extracted for each temperature. The results show a transition from damage-tolerant to failure-dominated behaviour as scratch severity, applied load and temperature increase. Mild pre-damage can be locally stabilised by debris compaction and oxide tribolayer formation, whereas deep pre-damage and high temperature promote delamination, substrate exposure and mechanically mixed oxides. At 800 °C, nine of 36 load pairs were free of unfavourable events; eight formed the conservative contiguous safe envelope, defined by two upper boundary points. The proposed framework goes beyond conventional adhesion or wear metrics by explicitly linking pre-existing damage to subsequent sliding response. Within the limits of a single structured design-grid campaign, the method provides a transferable screening concept for defect-sensitive tribological coatings in severe environments.
AB - High-temperature coatings are routinely exposed to pre-existing surface damage, yet their ability to sustain sliding contact after such damage remains insufficiently quantified. This study develops a damage-tolerant reliability-mapping workflow for AlCrN coatings deposited by physical vapour deposition (PVD), based on intersecting controlled pre-scratch defects with dry sliding contact at room temperature, 500 °C and 800 °C. A multilayer AlCrN coating on austenitic Cr-Ni-steel (253 MA) was first damaged by calibrated constant-load scratching (1.96–16.67 N) and then subjected to ball-on-disc sliding over an equivalent load range (temperature-dependent initial elastic Hertzian reference pressure 0.78–1.95 GPa). Surface responses at the scratch–wear intersections were classified using an 18-event taxonomy and reduced to a scalar reliability index; conservative monotone safe envelopes were then extracted for each temperature. The results show a transition from damage-tolerant to failure-dominated behaviour as scratch severity, applied load and temperature increase. Mild pre-damage can be locally stabilised by debris compaction and oxide tribolayer formation, whereas deep pre-damage and high temperature promote delamination, substrate exposure and mechanically mixed oxides. At 800 °C, nine of 36 load pairs were free of unfavourable events; eight formed the conservative contiguous safe envelope, defined by two upper boundary points. The proposed framework goes beyond conventional adhesion or wear metrics by explicitly linking pre-existing damage to subsequent sliding response. Within the limits of a single structured design-grid campaign, the method provides a transferable screening concept for defect-sensitive tribological coatings in severe environments.
M3 - Article
SN - 0257-8972
JO - Surface and Coatings Technology
JF - Surface and Coatings Technology
ER -