Depth-Dependent Young’s Modulus of Plasma-Sprayed Nickel: Experimental and Atomistic Insights

  • Robert Gordon University

Research output: Contribution to journal › Article › peer-review

3 Downloads (Pure)

Abstract

This study proposes a multiscale quantitative framework correlating experimentally measured depth-dependent Young’s modulus in plasma-sprayed nickel coatings with crystallographic stiffness limits obtained from molecular dynamics (MD) simulations along the [100], [110] and [111] orientations, using polycrystalline Ni as a comparative benchmark. Uniaxial tensile MD simulations were performed over a temperature range of 73 to 1000 K on nickel nanowires on different crystal orientations. At 300 K, the simulated Young’s modulus values were 136.3 GPa, 190.8 GPa and 245.4 GPa for the [100], [110] and [111] orientations, respectively, whereas the polycrystalline wire yielded a value of 139.4 GPa. Nanoindentation measurements conducted across the coating cross-section revealed a significant reduction in elastic modulus with increasing distance from the coating surface, from 211.1±4.7 GPa at through-thickness depth of 27 µm to 132.2±8.5 GPa at through-thickness depth of 200 µm. Correlative analysis suggests that the observed modulus gradient is consistent with the combined effects of coating architecture and microstructural variations. Plasticity in nickel nanowires was seen to arise from the nucleation of a/6⟨112⟩ Shockley partial dislocations, primarily from the free surface. As these partials glide on the {111} planes, they leave behind stacking faults. Interactions between partials moving on intersecting slip planes subsequently generate sessile a/6⟨110⟩ stair-rod dislocations at the junctions between stacking faults.
Original languageEnglish
Article number133805
JournalSurface and Coatings Technology
Volume536
Early online date27 Jul 2026
DOIs
Publication statusPublished - 15 Sept 2026