Abstract
This study investigates the use of alkali activated slag GGBS with dealuminated
metakaolin DK to produce mortars. Mortars composed of GGBS and DK were prepared and tested for 7-days compressive strength. With a fixed proportion of GGBS to DK 75%, 25%, three sets of mix designs were introduced each focusing on certain combinations of activators with different ratios. The first set tested mortars activated with sodium hydroxide SH and sodium silicate SS. The second set tested mortars activated with SH and sodium carbonate SC, and the third tested all the three activators. Results showed that mortars with lower modulus of silicate Ms=0.4 and Ms =0.2 and no SC showed higher compressive strength reaching around 45 MPa however suffering a very high flash setting, as compared to the higher moduli Ms=1.2 and Ms=0.8 where 25 MPa was recorded. Reasons are attributed to the high silica content in DK where lower Ms incorporates lower SS with lower silica which is compensated from the DK. In addition, mortars activated by SH and SC has shown also high compressive strength with different molar ratios reaching up to 50 MPa and delayed reaction, better workability with no flash setting. Finally, mortars activated with all the three activators showed a reduction almost by 50% in compressive strength. Reasons are also attributed to the introduction of the SS which increases the silica content.
metakaolin DK to produce mortars. Mortars composed of GGBS and DK were prepared and tested for 7-days compressive strength. With a fixed proportion of GGBS to DK 75%, 25%, three sets of mix designs were introduced each focusing on certain combinations of activators with different ratios. The first set tested mortars activated with sodium hydroxide SH and sodium silicate SS. The second set tested mortars activated with SH and sodium carbonate SC, and the third tested all the three activators. Results showed that mortars with lower modulus of silicate Ms=0.4 and Ms =0.2 and no SC showed higher compressive strength reaching around 45 MPa however suffering a very high flash setting, as compared to the higher moduli Ms=1.2 and Ms=0.8 where 25 MPa was recorded. Reasons are attributed to the high silica content in DK where lower Ms incorporates lower SS with lower silica which is compensated from the DK. In addition, mortars activated by SH and SC has shown also high compressive strength with different molar ratios reaching up to 50 MPa and delayed reaction, better workability with no flash setting. Finally, mortars activated with all the three activators showed a reduction almost by 50% in compressive strength. Reasons are also attributed to the introduction of the SS which increases the silica content.
| Original language | English |
|---|---|
| Publication status | Published - 14 May 2026 |
| Event | 17th International Conference on Civil and Architectural Engineering - Cairo, Egypt Duration: 11 May 2026 → 14 May 2026 Conference number: 17 |
Conference
| Conference | 17th International Conference on Civil and Architectural Engineering |
|---|---|
| Abbreviated title | ICCAE-17 |
| Country/Territory | Egypt |
| City | Cairo |
| Period | 11/05/26 → 14/05/26 |
Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver